TY - JOUR
T1 - Thermal decomposition mechanisms of phosphorus flame retardants
T2 - A combined theoretical and experimental approach
AU - Chen, Jiuke
AU - Lehner, Sandro
AU - Teng, Sin Yong
AU - Gaan, Sabyasachi
AU - Passerone, Daniele
AU - Heuberger, Manfred
AU - Gooneie, Ali
N1 - Funding Information:
This work was supported by the Empa-Internal Research Call in the framework of the \"ReFR\" project. Computational support from the Swiss Supercomputing Center (CSCS) under project ID s1276 is gratefully acknowledged (D. P. and J. C). We appreciate Dr. Arvindh Sekar, Dr. C\u00E9dric Hervieu, Dr. Rudolf Hufenus, and Dr. Wenyu Wu Klingler for their advice and support.
Publisher Copyright:
© 2025 The Author(s)
PY - 2025/11/1
Y1 - 2025/11/1
N2 - Phosphorus flame retardants (PFRs) are one of the main candidates for a fully organic, sustainable replacement to traditional halogenated FRs. However, their unexpected decomposition remains an open challenge hindering their full potential for sustainable applications in polymers. To address this issue, thermal decomposition of two common PFRs, namely 6H-Dibenz[c,e][1,2]oxaphosphorin, 6-[(1-oxido-2,6,7-trioxa-1-phospha bicyclo[2.2.2]oct-4-yl)methoxy]-, 6-oxide (DOPO-PEPA) and Aflammit PCO 900 (AF), was studied using density functional theory (DFT) coupled with experimental methods, particularly the direct inlet probe-mass spectrometry (DIP-MS). The DIP-MS spectra were processed and analyzed using algorithms to identify potential decomposition products of DOPO-PEPA and AF. Under inert atmospheric conditions, bond dissociation and proton attack were identified as the predominant decomposition pathways. Geometries of intermediates, transition states, and products along potential energy surfaces were identified through DFT calculations. For DOPO-PEPA, the dissociation of the C[sbnd]O bond linking the DOPO and PEPA moieties was identified as the most kinetically favored dissociation pathway; while for AF, bond dissociation was found energetically demanding. On the other hand, protonation processes demonstrate more dependence on the availability of protons. Cross-validating computational results with experimental observations verified the pathways through which DOPO-PEPA and AF release phosphorus-containing species and other decomposition products. Benefitting from a combination of fundamental molecular models and experimental evidence, this study provides new insights into the molecular mechanisms of thermal degradation of PFRs, thus providing a template for developing new FRs with enhanced thermal stability.
AB - Phosphorus flame retardants (PFRs) are one of the main candidates for a fully organic, sustainable replacement to traditional halogenated FRs. However, their unexpected decomposition remains an open challenge hindering their full potential for sustainable applications in polymers. To address this issue, thermal decomposition of two common PFRs, namely 6H-Dibenz[c,e][1,2]oxaphosphorin, 6-[(1-oxido-2,6,7-trioxa-1-phospha bicyclo[2.2.2]oct-4-yl)methoxy]-, 6-oxide (DOPO-PEPA) and Aflammit PCO 900 (AF), was studied using density functional theory (DFT) coupled with experimental methods, particularly the direct inlet probe-mass spectrometry (DIP-MS). The DIP-MS spectra were processed and analyzed using algorithms to identify potential decomposition products of DOPO-PEPA and AF. Under inert atmospheric conditions, bond dissociation and proton attack were identified as the predominant decomposition pathways. Geometries of intermediates, transition states, and products along potential energy surfaces were identified through DFT calculations. For DOPO-PEPA, the dissociation of the C[sbnd]O bond linking the DOPO and PEPA moieties was identified as the most kinetically favored dissociation pathway; while for AF, bond dissociation was found energetically demanding. On the other hand, protonation processes demonstrate more dependence on the availability of protons. Cross-validating computational results with experimental observations verified the pathways through which DOPO-PEPA and AF release phosphorus-containing species and other decomposition products. Benefitting from a combination of fundamental molecular models and experimental evidence, this study provides new insights into the molecular mechanisms of thermal degradation of PFRs, thus providing a template for developing new FRs with enhanced thermal stability.
KW - Dft calculations
KW - Mass spectrometry
KW - Phosphorus flame retardants
KW - Thermal decomposition
KW - Transition state theory
U2 - 10.1016/j.polymdegradstab.2025.111543
DO - 10.1016/j.polymdegradstab.2025.111543
M3 - Article
SN - 0141-3910
VL - 241
JO - Polymer Degradation and Stability
JF - Polymer Degradation and Stability
M1 - 111543
ER -